KQ Zinc 
 
• Advanced electric plating and quenching technology ensures the uniformity of zinc coating, it provides stable
  electrode discharge.
• The machining time saves 10%-20% than brass wire. 
• Good for auto-threading,suitable for 4 or over 4 cuts on hard metals.
APPLICABLE INDUSTRIES  
 
 
 
 
 
 
Product Series Core Material Coating Feature Tensile Strength N/mm² Elongation
(%)
Diameter Tolerence
(mm)
KQ Zinc 900 CuZn40 Zinc treated Hard:900   <3

0/-0.002 (0.20,0.25,0.30)

KQ Zinc 500 CuZn40 Zinc treated Soft:500 ≥3
Spool/Dia.
 (mm)
0.20  0.25  0.30 
P5  ★ ★ ★
P10 ★ ★ ★
P20 ★ ★ ★
K125 ★ ★ ★
K160 ★ ★ ★
K200 ★ ★ ★
K250 ★ ★ ★

Note: Blacked ones are standard specifications,strongly recommended.